Full metadata record
DC FieldValueLanguage
dc.creatorLlavori, I. (Iñigo)-
dc.creatorGiner, E. (Eugenio)-
dc.creatorZabala, A. (Alaitz)-
dc.creatorInfante-Garcia, D. (Diego)-
dc.creatorAginagalde, A. (Andrea)-
dc.creatorRodriguez-Florez, N. (Naiara)-
dc.creatorGómez-Mitxelena, X. (Xabier)-
dc.date.accessioned2024-01-12T12:37:17Z-
dc.date.available2024-01-12T12:37:17Z-
dc.date.issued2019-06-
dc.identifier.citationLlavori, I., Giner, E., Zabala, A., Infante-Garcia, D., Aginagalde, A., Rodriguez-Florez, N., & Gomez, X. (2019). Critical analysis of the suitability of crack propagation direction criteria for 2D cylindrical plain fretting contact. Engineering Fracture Mechanics, 214, 534-543.es_ES
dc.identifier.issn0013-7944-
dc.identifier.urihttps://hdl.handle.net/10171/68333-
dc.description.abstractIn this work the suitability of the criterion of maximum effective amplitude of the normal stress (Delta sigma(n,eff))(max) and the criterion of minimum shear stress range (Delta tau)(min) for 2D cylindrical plain fretting contact condition has been analysed. The numerical analysis has been performed by means of the extended finite element method, which takes into account the contact between crack faces during the closing part, and the results have been compared with experiments reported in the literature. Results show that overall the (Delta tau)(min) criterion predominates in intermediate stage, while the (Delta sigma(n,eff))(max) shows less deviation in the final stage. However, the predicted crack path by the latter criterion shifts toward the outer side, which do not correlate with the experimental results reported in the literature. Additional studies should investigate the variables that are affecting this change in the behaviour along the crack in order to set a criteria that is able to predict the plain fretting condition crack paths accurately.es_ES
dc.language.isoenges_ES
dc.publisherPergamon-Elsevier Science LTD.es_ES
dc.subjectCrack paths.es_ES
dc.subjectCrack propagation.es_ES
dc.subjectFrettinges_ES
dc.subjectExtend finite elements.es_ES
dc.titleCritical analysis of the suitability of crack propagation direction criteria for 2D cylindrical plain fretting contact.es_ES
dc.typeinfo:eu-repo/semantics/articlees_ES
dc.editorial.noteCC BY-NC-ND-
dc.identifier.doi10.1016/j.engfracmech.2019.04.035-

Files in This Item:
Thumbnail
File
CrackPath_postprint.pdf
Description
Size
1.62 MB
Format
Adobe PDF


Statistics and impact
0 citas en
0 citas en

Items in Dadun are protected by copyright, with all rights reserved, unless otherwise indicated.